u/Mental-Funny2590

Neptune 4 Max

Cura

Inland PETG-CF

250 Nozzle Temp, 80 Bed Temp

50mm/S first layer speed.

This is the first layer of the print.

Seems to lay down great everywhere but these locations. Non-adherence/tearing only happens on first layer. after these issues it will print with no issues.

Bed was automatically leveled and z height set with paper.

u/Mental-Funny2590 — 17 days ago