I'm having issues getting corners to come out right. Started going through Orcaslicer's calibration and this is what the pressure advance tower test came out as. I know the goal of this test is to find the right PA value, but per this print no value is good. How can I fix this?

Bambu P1S, 0.4 nozzle
Orcaslicer
Overture PETG white (brand new spool)
255 nozzle temp, 80 bed temp
This print would have ran at 200mm/s, though I've had issues as far down as 50mm/s
Retraction is defaulted at 0.8mm, 30mm/s