u/Flopi-Flop

Hi all !

I'm a recent owner of the Sovol SV08 (rooted with mainline Klipper).

I've done the calibration using OrcaSlicer calibration tests, but I'm still having one issue on my first few prints.

It seems that after bridging, and also after some sudden changes of directions, I have some under-extrusion.

Print settings :

  • Printer : Sovol SV08 (with TriangleLabes CHCB Hotend)
  • Slicer : OrcaSlicer
  • Filament : JAYO HS PETG (Blue)
  • Nozzle and bed temperature : 0.4 nozzle at 245°C / Bed at 80°C
  • Print Speed : Outer Wall 200mm/s, max acceleration at 4500mm/S2
  • Retraction : Distance 0.4, Z-Hop 0.4.
  • Pressure advance (calibrated with PA Pattern) : 0.035

Any idea what might be causing this ?

https://preview.redd.it/9b7qfou0j0yg1.jpg?width=1440&format=pjpg&auto=webp&s=91f2ae80730c3b465f04b0cfa49774126a8113f8

https://preview.redd.it/cx22yqu0j0yg1.jpg?width=1080&format=pjpg&auto=webp&s=570e5c879a2707613e38eb48cc02930c63dacca0

https://preview.redd.it/lyrlhmu0j0yg1.jpg?width=1080&format=pjpg&auto=webp&s=918e6666ae12cb7068b376df3bdedeefb717ee32

Thanks in advance !