P1S
PLA Matte from bambulab
220C and 55C bed
Normal speed (100%)
Bambulab studio for all slicing and so on

No matter what i do i get this wierd issue on the first 3 or so layers after that it’s fine, its also not on every object i print but it happens almost always, also the bed was recently washed

Im thinking this might be moist filament although its stored with silica dessicant in the AMS

u/AvidEnjoyer12 — 10 days ago